The main raw material for the sliding slab is aluminum-carrier and aluminum-cycle carbon. The need for special steel makes the development of a sliding slab of a variety. A brick from a sliding slab has advantages of high fire resistance, good chemical stability, resistance to corrosion of slag and liquid metals, good resistance to oxidation and refusing.
Physical and chemical indicators of a sliding plate
Physical and chemical indicators:
Subject | Index | |||
HBLT80 | HBLT75 | HBLT70 | ||
Al2O3 % | ≥80 | ≥75 | ≥70 | |
C % | ≥2 | ≥3 | ≥3 | |
Cold crush strength, MPa | Lack of impregnation | ≥80 | ≥70 | ≥60 |
Impregnation | ≥100 | ≥90 | ≥80 | |
Apparent porosity % | Lack of impregnation | ≤13 | ≤13 | ≤13 |
Impregnation | ≤10 | ≤10 | ≤10 | |
Bulk density, g/cm3 | Lack of impregnation | ≥2.9 | ≥2.85 | ≥2.75 |
Impregnation | ≥2.95 | ≥2.9 | ≥2.85 |
Aluminum Zirconium Carbon:
Subject | Index | ||||
Hbltg80 | HBLTG75 | HBLTG70 | HBMLT80 | ||
Al2O3 % | ≥80 | ≥75 | ≥70 | / | |
Al2O3+MgO % | / | / | / | ≥80 | |
C % | ≥3 | ≥3 | ≥4 | ≥3 | |
ZrO2 % | ≥4 | ≥4 | ≥4 | / | |
Apparent porosity % | Lack of impregnation | ≤13 | ≤13 | ≤13 | ≤13 |
Impregnation | ≤10 | ≤10 | ≤10 | ≤10 | |
Bulk density, g/cm3 | Lack of impregnation | ≥3.0 | ≥2.95 | ≥2.9 | ≥2.75 |
Impregnation | ≥3.05 | ≥3.0 | ≥2.95 | ≥2.8 | |
The strength for crushing in the cold state of MPa | Lack of impregnation | ≥90 | ≥90 | ≥80 | ≥70 |
Impregnation | ≥110 | ≥110 | ≥100 | ≥90 |